Substrate Type | Woven fiberglass ( “E” type) |
---|---|
Coating Medium | Polytetrafluoroethylene |
Coated Weight
(nominal) |
0.800 (pounds/sq.yard)
434.0 (grams/sq.meter) |
Overall Thickness
(nominal) |
0.008 (inches)
0.2032 (mm) |
Operating Temperature | -100°F to 500°F (continuous)
-73°C to 260°C |
Tensile Strength (warp/fill)
(nominal) |
260 / 160 (pounds/inch of width)
2276 / 1401 (Newtons/5cm) |
Tear Strength (warp/fill)
(nominal) |
14.00 / 7.00 (pounds-f) (trapezoid method)
62.25 / 31.15 (Newtons) |
Dielectric Strength
(nominal) |
650 (volts/mil) |
Adhesion (warp/fill)
(nominal) |
4.70 / 4.80 (pounds/inch of width) (resin to substrate)
41.15 / 42.02 (Newtons/5cm) |